What a usable record contains
| Item | Why |
|---|---|
| Weld number | The only reliable link to the log and the map |
| Date and inspector | Who examined it and when |
| Images covering the circumference | One image of one side does not show the whole bead |
| Result and reason | Accept or reject against the stated criteria |
| Equipment ID | Which borescope; for calibration or quality questions |
| Link to repair | If rejected, the repair weld number and its images |
Image quality rules
- Lighting and focus good enough to judge discoloration, bead width and penetration.
- The weld number visible in the image or in a fixed file name, not only in someone’s memory.
- No cropping or editing of images used for acceptance.
- Same viewing method each time, so images can be compared.
- Reference images of acceptable and rejectable welds, agreed with the owner, kept for inspectors to compare against.
Check the borescope itself as part of the record. A scratched lens, poor light or a probe that cannot reach the full weld produces images that cannot be judged. Note the equipment used, keep it clean, and replace or repair it when image quality drops, before an owner reviewer rejects a batch of records.
Naming and storage
Use a fixed naming pattern built from system, line and weld number, store images in the folder structure the turnover package will use, and back them up. A borescope image that cannot be found when the owner asks is little better than no image. Link the image reference in the weld log (weld maps and logs).
Where the owner spec decides
Owner specifications for semiconductor gas and chemical lines decide whether every weld or a sample needs borescope examination, the visual criteria (often based on SEMI F81) and the hand-over format. Some require images of sample welds as well as production welds. Retention after handover is also the owner’s call. Ask for these requirements before the first weld.
Sample and coupon welds deserve the same care. Where the owner requires start-of-shift or change-of-setup sample welds, their images show that the setup was right before production welding, and auditors may ask for them alongside the production weld images.
Hiring for it
Visual and borescope inspection is among the QA/QC skills WELDK’s capabilities page lists. Ask candidates how they named and stored images on their last job and test their judgement with real images (QA/QC interview questions). Defects you will see in the images are explained in common orbital weld defects.