Steps
- Report to the supervisor and QA; keep the section isolated.
- Help locate the source: recent joints, open-ended periods, components installed from damaged bags.
- Follow the rework plan the owner or QA approves.
- Reassemble with new gaskets and clean components.
- Retest and recertify as the specification requires.
| Finding | Possible source |
|---|---|
| Particles | Cutting debris, open ends, damaged component packaging |
| Moisture | Line left open, poor purge |
| Oxygen | Leak, poor purge |
| Discoloured welds found on inspection | Weld purge problems (weld defects) |
Learn from it
Brief the crew on the cause and change the routine that allowed it, for example capping rules or cutting methods (bagging and capping).